Mixing Low Cement Castables

 

  1. Clean the working area as well as other tools and equipment including the pan mixer, vibrator, tub and shovel so that no foreign substances can contaminate the refractory material.
  2. Don’t overload the mixer. In cases where castable containing separated binder is used, add one packer of binder per bag. Ensure that the binder is spread around the refractory material.
  3. Dry mix the castable for approximately one minute.
  4. To begin a mix, pour the smallest recommended amount of clean water into the mixer. Then add the balance of water required in small increments. Since water content is critical to the physical properties of the castable, do not use more than the recommended amount of water.
  5. Mix the material thoroughly for 2-3 minutes. Avoid mixing for longer than 5 minutes since this will generate hear and speed up the setting time.
  6. Before use, it is advisable to test the dense castable for proper consistency by shaking one handful of the material. Properly mixed castable should form into a lump with a glossy surface, and not flow through the fingers or break apart.
  7. The castable should be used immediately after being mixed. The time between mixing and casting should never exceed 30 minutes.

Mixing Precautions

  1. Check the tools and equipment to ensure their proper functioning
  2. The refractory material or equipment contaminated with cement or hardened castable can cause flash setting.
  3. A flash setting may result if the mixing takes place in a temperature higher than 25c-30c (the ambience temperature), or if the temperatures of the castables, the water or equipment are too high. It, therefore, is important that the material and equipment should not be left in the sun for a lengthy period of time before use.
  4. The water used in mixing the castable must be clean and have a neutral ph.
  5. Too much water in the mix can cause many undesired effects. Among them are slow setting, reduced mechanical strength, high porosity, and high risk of explosion during the heat-up at very high temperatures.
  6. A flash setting and reduced physical bond may result from insufficient water in the mix